This analysis is available for identification of the corrosion/ failure mechanism, i.e. pitting corrosion, stress corrosion cracking, microbiologically infl uenced corrosion, galvanic corrosion, etc. of failed sprinkler pipe. The analysis involves removing a section of the the failed pipe from the fi re sprinkler system and sending to a certifi ed third party lab for testing. Material fl aw/quality evaluations will be made to determine potentially related factors to the failure condition. This will include metallographic examination for microstructural fl aws or abnormalities.
The methods used in the failure / corrosion analysis will typically include visual examination, examination by optical microscopy, examination by scanning electron microscopy (SEM), metallographic examinations (cross sectional examination of material microstructure), energy dispersive spectroscopy (EDS) of corrosion products/residues, microbiological activity studies, hardness survey and chemical analysis.
A formal report, with photographic documentation will be generated upon completion approximately 15 business days after the test is started.
1119183 Specifications PDF
Product Reviews
Write your own review
Rate this product: